Gịinjection ịkpụzi ịghasa gbọmgbọmna-ekpebi ogo agbaze, ịgbatị agbaze, na oge okirikiri. N'okpuru: otu esi ahọrọ geometry na ọgwụgwọ elu maka resin gị, otu esi echekwa setịpụ, yana otu esi achọpụta ntụpọ azụ na skru, gbọmgbọm, ma ọ bụ mgbanaka nlele kama ịchụ ya site na ntọala igwe. Anyị nitrided 38CrMoAlA injection skru na-ebu 0.5–0.8 mm nitrided oyi akwa na 950–1050 HV, suit PE, PP, PS, na ABS, na ijikwa eriri iko ruru 30%. N'oge gara aga, ma ọ bụ na resin na-emebi emebi, olulu ahụ chọrọ ịfesa alloy siri ike ruo 62 HRC. Ọ bụrụ na mmepụta adalata wee gbatịa okirikiri, gụọ tebụl nhụsianya tupu ị metụ ntọala ọzọ aka.

Injection molding screw barrel set manufactured by Nanhaiya screw barrel factory

Kedu ihe bụ ogbugba mkpụzi screw Barrel?

Ihe ịghasa na gbọmgbọm ahụ na-etolite akụkụ plasticizing nke igwe na-akpụzi injection. Ha na-ejikọta ọnụ, na-ewere pellets siri ike na hopper, gbazee ha, gwakọta ha ka ọ bụrụ otu agbaze, mita otu égbè, ma gbanye nke ahụ n'ime ihe ahụ. Akụkụ ọ bụla igwe gị na-emepụta na-agafe ụzọ abụọ a.

Ndị na-akpụ akpụ na-edochi nozzles, na-akụ ihe ndị na-akpụ akpụ, ma na-edozi okpomọkụ ruo izu ole na ole tupu ha eleba anya na ngalaba plasticizing. Usoro ahụ bụ azụ azụ. Mgbe ịghasa ma ọ bụ gbọmgbọm ahụ na-eyi, ọ nweghị ntọala dị na njikwa na-eweghachi usoro a azụ.

Ọrụ nke Screw na Plasticization

Ihe nkedo na-eme ọtụtụ n'ime agbaze, ọ bụghịkwa na ndị na-ekpo ọkụ. Okpomọkụ gbọmgbọm na-enye aka, mana usoro mgbaze kachasị bụshiee okpomọkụ: ịghasa na-adọkpụrụ polymer megide mgbidi gbọmgbọm ọkụ, esemokwu ahụ na-ebute okpomọkụ n'ime ihe ahụ n'onwe ya. Ọ bụ ya mere screw geometry ji agbanwe okpomoku agbaze ọbụlagodi mgbe ntọala ntọala gị anaghị akwagharị.

Ihe nkedo ahụ na-agbakwa mita agba. Ọ na-atụgharị ka ọ bụrụ plastik, na-atụgharị ka agbaze na-anakọta n'ihu ọnụ ọnụ, wee kwụsị. Ebe ọ na-eweghachi bụ nha ogbugba gị. Agbaze ọ bụla nke na-adaghachi azụ n'elu ụgbọ elu ma ọ bụ gafere mgbanaka nlele na-emebi nha ahụ.

N'ikpeazụ, ịghasa injects. Ọ na-akwụsị ịtụgharị ma na-aga n'ihu dị ka onye na-akụ mmiri, na-amanye agbaze site na nozulu. Ọrụ abụọ a, na-atụgharị ma na-atụgharị, na-ekewa screw injection na skru extrusion.

Ọrụ nke gbọmgbọm na nnyefe ọkụ na njide

gbọmgbọm ahụ bụ arịa nrụgide ziri ezi nke nwere ọkụ ọkụ. Ọ nwere nrụgide injection, na-ebufe okpomọkụ site na eriri n'ime polymer, ma na-enye mgbidi siri ike nke ịghasa na-akwa ihe megide ya.

Ọkpụkpụ ya kwesịrị ịdị okirikiri, kwụ ọtọ na nke siri ike. Mgbe olulu ahụ na-eyi oversize, nkwụsị n'etiti ụgbọ elu ụgbọ elu na mgbidi gbọmgbọm na-eto. Agbaze wee na-awụpụ azụ azụ n'elu ụgbọ elu kama ịga n'ihu, ọnụ ọgụgụ plasticizing dara.

A na-ekewa ikpo ọkụ Barrel, na-abụkarị nri, mkpakọ, na mita, nke ọ bụla nwere njikwa nke ya na thermocouple. Igwe ọkụ ọkụ na-efegharị efegharị n'otu mpaghara nwere ike esi nri ruo ọnwa ole na ole ka ihe ngosi na-agụkwa nke ọma.

Kedu ka Screw na Barrel si arụkọ ọrụ dịka Sistemu

Akụkụ abụọ a na-arụ ọrụ dị ka ụzọ jikọtara ọnụ, ọnụọgụ na-akọwa ụzọ abụọ ahụ bụmkpochapụ radial: ọkara ọdịiche dị n'etiti gbọmgbọm gbara dayameta na ịghasa dayameta ụgbọ elu.

Nchapụta dị ntakịrị site na imewe. Ụkpụrụ isi mkpịsị aka ụlọ ọrụ maka nhazi ọhụrụ bụ ihe dị ka 0.001 inch nke mkpochapụ n'otu akụkụ maka inch ọ bụla nke skru dayameta. Na skru 60 mm (ihe dị ka 2.36 in), nke ahụ na-agbada nso 0.06 mm kwa akụkụ. Ịse ihe owuwu gị bụ ikike, ọ ga-abụkwa nọmba ị na-enyocha megide ya.

Obere oghere ahụ na-arụ ọrụ n'ezie. Ọ na-amanye polymer ịkwa akwa na mgbidi gbọmgbọm kama ịgafe. Ugboro abụọ na mkpochapụ na ncha ahụ na-ada mbà, na-agbaze nwayọọ nwayọọ, mmepụta na-adaba, na igwe na-anwa ịkwụ ụgwọ na okpomọkụ ọ na-ekwesịghị ịdị mkpa.

Dochie otu akụkụ naanị ya anaghị esiri ike idozi otu ụzọ eyiri. Mkpọsa ọhụrụ dị n'ime gbọmgbọm eyi uwe na-eweghachi nanị ọkara nke furu efu, na ndakọrịta na-eyi akụkụ ọhụrụ ahụ ngwa ngwa karịa ka o kwesịrị.

Anatomi nke Injection Molding Screw

Ọkọlọtọ ogbugba ogbugba na-ekewa n'ime mpaghara atọ yana mgbakọ ọnụ. Mpaghara ọ bụla nwere ọrụ, nke ọ bụla na-adakwa n'ụzọ ị nwere ike ịmata.

Mpaghara Ọwa omimi Job Kedu ọdịda dị ka
Nri miri emi Were pellets, bufee ha n'ihu Ịchịkọta, agụụ, nri na-adịghị agbanwe agbanwe, mgbake na-ekwekọghị ekwekọ
Mkpakọ (ngbanwe) Na-emighị emi Kọmpat na gbazee polymer megide mgbidi gbọmgbọm Adịghị agbaze, ngwakọta adịghị mma, mpaghara a na-eyi mbụ
Mita Na-emighị emi Homogenize na gbapụta agbaze na-agbanwe agbanwe Mgbanwe agbapụ, mmụba okpomọkụ
Ndụmọdụ na lelee mgbanaka — Mechie ihe mgbochi azụ n'oge ịgba ntụtụ Mfefe nha nke mgbọ, mkpirisi mkpirisi, mfu nkuchi

Mpaghara nri

Ọwa dị omimi na-ejide pellets site na akpịrị hopper wee na-aga n'ihu dị ka ihe siri ike. Mpaghara a anaghị agbaze nke ukwuu. Ọ na-enyefe.

Nsogbu nri na-eme ka nsogbu na-agbaze. Ọ bụrụ na pellets na-agafe na akpịrị, ma ọ bụ akụkụ nri na-ekpo ọkụ nke ukwuu ma pellet na-adị nro ma rapara n'isi n'isi, agụụ na-agụ ya. Oge mgbake na-agbanwe, na nha agba na-esote. Lelee nri-akpịrị jụrụ oyi tupu ị taa ụta geometry.

Mpaghara mkpakọ (Transition).

Ọwa na-akawanye omimi n'akụkụ a. Nke ahụ na-emighị emi na-amanye polymer megide mgbidi gbọmgbọm na-ekpo ọkụ ma na-ebute okpomọkụ nke na-eme ka ọ gbazee.

Mpaghara mkpakọ bụ ebe uwe na-etinye uche. Nrụgide na-arị elu ebe a, na ihe ndị na-ekpo ọkụ na-ekpo ọkụ na-egweri ebe a. Mgbe ị tụrụ ihe nkedo eyi, nke a bụ ebe mbụ ị ga-ahụ ọnụọgụgụ.

Mpaghara mita

Ọwa na-emighị emi, nke dị omimi mgbe niile na-eme ka mgbaze ahụ na-agbaze ma na-ebufe ya n'ihu na nrụgide na-adịgide adịgide. Mpaghara a na-ekpebi nkwụsi ike nke agba na-agba.

Mwepụta nke mpaghara-mita na-egosi dị ka mgbanwe agba na ịrị elu okpomọkụ n'otu ebe. Ihe nkedo ahụ na-agbasi mbọ ike ibugharị otu ihe ahụ.

Ntuziaka skru, Lelee mgbanaka & Valve anaghị alaghachi azụ

Mgbakọ mgbanaka nlele, mgbe ụfọdụ a na-akpọ valvụ na-adịghị alaghachi azụ, kwesịrị nlebara anya karịa ka ọ na-enweta. Ọ na-anọdụ n'ọnụ ọnụ ịghasa ma na-arụ otu ọrụ: n'oge injection ọ na-emechi, ya mere agbaze na-abanye n'ime ihe kama azụ n'elu ịghasa.

Mgbe ọ kwụsịrị akara, ị ga-enweta mgbanwe nha nha nha, mkpụkpọ mkpirisi, na ihe nkuku na-apụ n'anya. Ndị na-akpụ akpụ na-eji izu na-edozi nrụgide injection, ijide oge na okpomọkụ na-achụ nke a. Ọ dịghị nke ọ bụla na-arụ ọrụ, n'ihi na agbaze na-agbanarị azụ n'ofe mgbanaka eyi.

Mgbama atọ na-atụ aka na mgbanaka nlele kpọmkwem. Nkuku na-adịgasị iche ịba agba karịa ka ọ na-anọ mgbe niile. Arọ gbara agba na-efegharị mgbe igwe na-akọ mgbake nkịtị. Na usoro a na-emegharị ugboro ugboro na-atụgharị na mberede na-enweghị mgbanwe na resin ma ọ bụ ntọala.

Nchọpụta nyocha bara uru nkeji iri:Ọ bụrụ na nha ogbunigwe gị na-awagharị ma nkuku adịghị ekwekọ, lelee mgbanaka nlele tupu imetụ ntọala ọzọ aka. Mgbanaka ahụ na-eyi ngwa ngwa karịa ịghasa, na-akwụ ụgwọ dị nta nke skru, ma na-edochi ya karịa ọtụtụ oge nhazi nhazi.

Parameters igodo ịghasa geometry

Ọnụọgụ anọ na-akọwa ihe nkedo injection. Ghọta ha, na ntinye nke onye na-ebubata ya kwụsịrị ịbụ igbe ojii.

Oke L/D: Nkọwa, usoro na ụkpụrụ akwadoro site na resin

Oke L/Dbụ ogologo ọrụ nke ịghasa kewara ya n'obosara dayameta. Ihe nkedo ugboro 22 n'ogologo karịa obosara nwere L/D nke 22:1. A na-ekewa usoro a nke ọma site na D, yana nha nha nha: skru 50mm na 22:1 nwere ogologo ọrụ 1,100mm.

L/D na-achịkwa ọnụ ụlọ nke ịghasa ga-agbaze, gwakọta, na homogenize. Ogologo oge na-enyekwu ikike ịgbaze na ngwakọta ka mma. Mkpirisi na-enye obere oge obibi, nke na-echebe resins nwere mmetụta okpomọkụ.

Ihe nkedo injection na-adị mkpụmkpụ karịa skru extrusion. Ihe ịghasa na-akwado otu ogbunigwe n'otu oge kama ịgbapụta mmiri na-aga n'ihu, ihe onwunwe na-anọdụkwa na gbọmgbọm n'etiti gbaa. N'imeỊkpụzi nha nha L/Domume, ọtụtụ igwe na-ada n'etiti 18:1 na 25:1, na 20:1 ka 22:1 nkịtị na n'ozuzu-ebumnobi igwe.

Resins na-ekpo ọkụ na-ekpo ọkụ dị ka PVC na-akwado njedebe dị mkpirikpi, ya mere ihe onwunwe na-eji obere oge na-ekpo ọkụ. Plastics injinia nke chọrọ ịgbaze nke ọma na-akwado njedebe dị ogologo. Ntuziaka nha L/D anyị na-ekpuchi azụmaahịa n'ime omimi.

Oke mkpakọ: Otu o si emetụta ikpo ọkụ yana ogo agbaze

Oke mkpakọna-atụnyere omimi nke ọwa na mpaghara nri na omimi nke ọwa na mpaghara mita. Ihe nkedo nwere ọwa ndepụta dị omimi okpukpu atọ karịa ọwa mita ya nwere oke mkpakọ nke 3:1.

Oke mkpakọ na-esetịpụ ka ịghasa si arụ ọrụ ihe. Mkpakọ dị elu pụtara ịkwa akwa karịa, okpomoku arụrụ arụ, yana mgbaze na-eme ihe ike. Mkpakọ ala na-emeso polymer nke ọma.

Dakọtara ya na resin, ọ bụghị na mmasị maka ọnụọgụ buru ibu. Polyolefins nwere obere viscosity chọrọ mma shiee ka ọ gbazee nke ọma. Resins nwere mmetụta na-ekpo ọkụ dị ka PVC, PC, na POM na-emebi emebi n'okpuru shiee nke PE ga-ewepụ. Ntuziaka oke mkpakọ anyị na-arụ ọrụ site na oke.

Omimi ụgbọ elu, obosara ọwa, na mmetụta ha na mmepụta

Oke mkpakọ bụ oke, na skru abụọ nwere otu oke nwere ike ịkpa àgwà dị iche iche. Ihe omimi zuru oke dị mkpa.

Ọwa nyocha dị omimi na-ebugharị ihe ndị ọzọ kwa mgbanwe, na-ebuli ọnụego plasticizing, mana ọ na-agwakọta nke ọma ma na-ewepụta obere agbaze. Ọwa mita na-emighị emi na-agwakọta nke ọma ma na-ebuga ọnọdụ okpomọkụ na-agbanwe agbanwe, na mmepụta dị ala n'otu oge.

Obosara ụgbọ elu na akụkụ helix na-emetụta ọrụ mbufe na ncha ihe a na-ahụ na ala ụgbọ elu. Ndị a bụ nkọwa nhazi nke ị na-akọwapụta site na ịkọwa usoro gị na onye na-emepụta ihe screw, ọ bụghị ọnụọgụgụ ị ga-esi na tebụl.

Ịkpọ dayameta na mmekọrịta nke gbara agba

Dayameta nke ịghasa na-esetịpụ ikike ịgba egbe nke igwe. Ihe nkedo buru ibu na-ewepụ ụda karịa kwa milimita nke njem n'ihu, ya mere ọ na-ebuga nnukwu agba.

Iwu bara uru bụ eriri nkasi obi, ọ bụghị oke siri ike. Gbaa ogbunigwe nke na-eji obere akụkụ nke ikike gbọmgbọm ahụ na ihe ahụ na-anọdụ ala n'ime gbọmgbọm ogologo oge, na-agba ọsọ site na okpomọkụ ma na-eweda ya ala. Na-agba ọsọ n'ihe fọrọ nke nta ka ọ bụrụ ike zuru oke ma ị ga-efunahụ ihe dị mkpa maka mbukota na-agbanwe agbanwe.

Ọtụtụ ndị na-akpụ akpụ na-achọ mgbọ egbe n'etiti ebe a na-eji gbọmgbọm eme ihe. Ọ bụrụ na akụkụ gị na-anọdụ ala n'èzí eriri ahụ, ndozi ziri ezi bụ dayameta skru dị iche, ọ bụghị ntọala igwe siri ike.

Nke a bụ tebụl akụkụ anyị ebipụtara, nke na-egosi ka ikike ịgba égbè si agba ọsọ na nha gbọmgbọm gafere ebe anyị na-ewu. Jiri ya chọta igwe gị, ma ọ bụ iji chọpụta ịdị ọcha-elele dayameta nke ndị na-ebubata ya na-ehota gị.

Agba (g) Ịghasa Ø × ogologo (mm) Ogologo Barrel Ø × (mm)
30–90 Φ30 × 900 Φ85 × 860
60–125 Φ35 × 910 Φ85 × 860
100–150 Φ38 × 935 Φ95 × 900
125–160 Φ40 × 980 Φ95 × 910
125–300 Φ42 × 1030 Φ105 × 1110
250–400 Φ45 × 1210 Φ115 × 1165
300–500 Φ50 × 1300 Φ125 × 1260
450–600 Φ55 × 1335 Φ130 × 1320
500–700 Φ56 × 1350 Φ130 × 1350
500–700 Φ60 × 1380 Φ140 × 1350
650–800 Φ65 × 1415 Φ150 × 1420
700–1000 Φ70 × 1790 Φ160 × 1685
80–125 Φ75 × 1825 Φ170 × 1725
100–150 Φ80 × 2000 Φ180 × 1805
125–200 Φ85 × 2300 Φ190 × 1900
200–300 Φ90 × 2700 Φ210 × 2000
250–500 Φ100 × 2600 Φ230 × 2405
300–600 Φ110 × 2600 Φ256 × 2590
400–1000 Φ120 × 2800 Φ256 × 2800
600–800 Φ130 × 3010 Φ256 × 2970
800–1000 Φ145 × 3010 Φ256 × 3200
1000-1500 Φ160 × 3500 Φ270 × 3200
1300-2500 Φ170 × 3415 Φ317 × 3380

Ihe abụọ a ga-agụ na ya. Ikike gbara agba na-arịgo na dayameta, dị ka physics chọrọ. Na gbọmgbọm dị n'èzí na-eto eto na ya, nke mere na nnukwu ịghasa anaghị abụ nkwalite n'efu: ọ bụ klas nha igwe dị iche.

Ụdị skru nke injection injections: Kedu nke ị chọrọ?

Ezinaụlọ ise na-ekpuchi ihe fọrọ nke nta ka ọ bụrụ ngwa ịgba ọgwụ ọ bụla. Nke ziri ezi dabere na resin gị na ihe akụkụ gị chọrọ.

Ụdị ịghasa Ihe ọ na-eme Kachasị mma maka Adịghị ike
Ebumnuche izugbe (GP) Otu ụgbọ elu, mpaghara atọ ọkọlọtọ PE, PP, PS, ABS, ọtụtụ resins ngwa ahịa mebie geometry; na-alụ ọgụ na-achọ resins
Ihe mgbochi Ụgbọ elu nke abụọ na-ekewa akwa siri ike na ọdọ mmiri gbazee Mgbaze ka mma, mmepụta dị elu, akụkụ ndị na-adịghị agbaze Na-eri ihe; overkill na mfe resins
Ngwakọta / ngwakọta Na-agbakwunye akụkụ Maddock ma ọ bụ pin Agba masterbatch, ogige jupụtara, akụkụ nwere mmetụta streak Ịkwa akwa ọzọ; ezighi ezi maka resins nwere mmetụta okpomọkụ
Vented (ogbo abụọ) Mpaghara nkwụsịtụ yana ọdụ ụgbọ mmiri ikuku na-ewepụ ihe na-agbanwe agbanwe Hygroscopic resins ebe ihicha na-abaghị uru Mgbagwoju anya; ikuku nwere ike ịdaba ma ọ bụrụ na ejikọtaghị ya
PVC kpọmkwem Mkpakọ dị ala, ebe a na-egbu maramara, enweghị ntụpọ nwụrụ anwụ PVC siri ike ma na-agbanwe agbanwe Ebumnuche-wuru; ọ bụghị ihe nkedo ebumnuche izugbe

Nzube izugbe (GP) Screw: Kachasị, Kasị Mma maka?

Ihe mkpuchi GP bụ nkwekọrịta, yana nke dị mma. Ọ na-agba PE, PP, PS, na ABS nke ọma, nke na-ekpuchi ọtụtụ ịkpụzi ngwa ahịa. Ndị na-ewu igwe na-ebuga ya dị ka ọkọlọtọ n'ihi na ọ bụ ndabara kacha dịrị nchebe mgbe ha amaghị ihe ị ga-agba.

Nkwekọrịta ahụ na-efu gị mgbe resin na-achọsi ike. Ihe GP skru na naịlọn jupụtara ugo na-eyi ngwa ngwa. Ihe nkedo GP na PVC siri ike na-eweda ihe ahụ ala. Ihe nkedo GP a na-akwali maka mmepụta kachasị na akụkụ mgbidi dị mkpa na-ewepụta ihe na-agbaze. Mgbe nke ọ bụla n'ime ihe ndị ahụ na-akọwa usoro gị, screw e wuru na-akwụ ụgwọ maka onwe ya naanị.

Mgbochi mgbochi: Nkewa na-agbaze ka mma na ịdị n'otu

Ihe mgbochi mgbochi na-agbakwunye ụgbọ elu nke abụọ site na mpaghara agbaze. Ụgbọ elu ahụ n'ụzọ anụ ahụ na-ekewapụ pellets siri ike fọdụrụ na gbazee nke etolitelarị, ma na-eme ka ihe siri ike nagide mgbidi gbọmgbọm dị ọkụ ebe ha na-aga n'ihu na-agbaze.

Na-enweghị ihe mgbochi, ihe siri ike na-ezo n'ime ọdọ mmiri gbazee, kpuchie ya na mgbidi, ma nwee ike ịlanarị ruo n'ọnụ mmiri ka ọ na-agbaze. Na otu, agbaze na-agwụcha kpamkpam na karịa mgbe niile.

Nkwụghachi ụgwọ ahụ ka mma gbazee otu n'otu ma ọ bụ mmepụta dị elu, nke na-egosi na ọ bụ ntakịrị ihe na-adịghị agbaze, njikwa ọkụ siri ike, na windo usoro sara mbara. Ndị na-akpụ akpụ na-eji nkwakọ ngwaahịa dị obere, akụkụ anya, ma ọ bụ ihe ọ bụla na-enweghị mgbaze kwesịrị ịrịọ otu aha.

Ngwakọta / Ngwakọta skru: Maka Ngwa Masterbatch juru na agba

Ngwakọta skru na-agbakwunye ngalaba ngwakọta raara onwe ya nye, na-adịkarị nso n'ọnụ. Akụkụ Maddock (fluted) na-amanye gbazee site na oghere dị warara, na-agbaji ihe ndị na-agbazeghị site na shii. Ndị na-agwakọta ntụtụ na-ekewa ma na-ejikọta eruba ahụ, na-ekesa agba na ndochi.

Jiri otu mgbe streaking agba bụ nsogbu dị mma, mgbe masterbatch mgbasa ihe dị mkpa, ma ọ bụ mgbe nkesa filler na-arụ ọrụ akụkụ. A na-agbakwunye ahịa ahia ahụ, nke na-eme ka ngwakọta ahụ bụrụ nhọrọ na-ezighị ezi maka resins na-ekpo ọkụ nke dịlarị nso na njedebe mmebi ha.

Ihe mkpuchi ventilashị / Degassing: Maka Resin Hygroscopic

Ihe mkpuchi ikuku na-agba ọsọ nkebi abụọ. Oge nke mbụ gbazee, mgbe ahụ ọwa na-emikpu na mberede, na-agbada nrụgide mgbaze na nso efu na ọdụ ụgbọ mmiri ikuku na-egbutu n'ime gbọmgbọm ahụ. Mmiri na ihe na-agbanwe agbanwe na-agbapụ n'ebe ahụ, na-adịkarị n'okpuru oghere. Nke abụọ ogbo wee repressurizes agbaze maka ịgba ogwu.

Nke a na-arụ ọrụ maka resins hygroscopic ebe ihicha na-abaghị uru ma ọ bụ nke a na-apụghị ịdabere na ya. Ọ na-ebukwa ihe ize ndụ: ọ bụrụ na usoro abụọ ahụ adabaghị, gbazee na-apụ na ọdụ ụgbọ mmiri kama gas. A ghaghị imekọ ihe nkedo ikuku na gbọmgbọm ikuku gbakọrọ ọnụ, nke mere e ji kọwaa ha dị ka nhazi na anaghị emegharị ya na mberede.

Ihe mkpuchi PVC akọwapụtara: Ihe kpatara skru ọkọlọtọ ji ada PVC

PVC siri ike na-ata ụta ọkọlọtọ n'ụzọ abụọ n'otu oge. Ọ na-eweda n'okpuru shiee, na-ahapụ hydrogen chloride, nke na-emebisị ígwè ọ nọ ọdụ megide. Mmebi amalite tupu onye ọrụ ahụghị ntụpọ.

Ihe mkpuchi PVC na-aza egwu abụọ ahụ. Mkpakọ dị ala na-eme ka ọ dị nro. Ebe a na-egbu maramara na geometry na-enweghị ntụpọ na-akwụsị ihe na-akwụsị ịnọ na-esi nri. Ntọala ahụ fọrọ nke nta ka ọ bụrụ mgbe niile chọrọ nguzogide corrosion na ọgwụgwọ elu, ọ bụghị naanị na-eyi nguzogide. AnyịPVC ịghasa gbọmgbọm nduna-ekpuchi kemịkalụ, na anyịconical ejima ịghasa orùjee ozi PVC n'akụkụ extrusion.

Iwu PVC na-echekwa barel:ahapụla PVC ka ọ nọ ọdụ na-ekpo ọkụ na igwe kwụsịrị. Sachapụ ya tupu nkwụsị ọ bụla ga-adịru. PVC kwụ ọtọ na-ekpo ọkụ na-eweda ala, acid ọ na-ewepụta na-awakpo oghere ahụ ka igwe na-anọdụ ala n'enweghị ọrụ.

Otu esi ahọrọ gbọmgbọm ịsa ahụ ziri ezi maka resin gị

Nhọrọ resin na-eme mkpebi ọ bụla ọzọ na ibe: geometry, ígwè na elu. Gụọ tebụl, wee gụọ ihe ndetu n'okpuru ya, n'ihi na ihe ndetu na-ebu ịdọ aka ná ntị.

Resin L/D a na-ahụkarị Oke mkpakọ a na-ahụkarị Ụdị ịghasa Ihe ndetu pụrụ iche
PP / PE 20:1–22:1 2.5:1–3.5:1 GP ma ọ bụ mgbochi Ịgbaghara. Achọrọ mma shiee ka ọ gbazee nke ọma
PS / HIPS 20:1–22:1 1.8:1–2.5:1 GP Ala viscosity, agbaze ngwa ngwa. Ngwakọta dị nro na HIPS
ABS 20:1–24:1 2.0:1–2.5:1 GP ma ọ bụ mgbochi Amorphous. Lelee ikpo ọkụ, streaks na-egosi n'ụzọ dị mfe
PC na injinia plastik 22:1–25:1 2.0:1–2.5:1 Ihe mgbochi ma ọ bụ GP, obere shiee Okpomọkụ gbazere dị elu, windo dị warara. L/D dị ogologo, mkpakọ dị nro
PVC siri ike 18:1–20:1 1.6:1–2.5:1 PVC kpọmkwem Nguzogide corrosion abụghị nhọrọ. Obere oge obibi
PVC mgbanwe 18:1–20:1 2.0:1–2.8:1 PVC kpọmkwem Na-agbaghara karịa onye isi ike, ka na-emebi emebi
PET (nke mbụ) 20:1–24:1 Nleta dị ala, nke ziri ezi Ebumnobi wuru PET Kpochapụ ya ma ọ bụ wetuo ya. Ọkpụkpụ dị ala, ebe obibi pere mpe, ebe a na-egbu maramara
POM (acetal) 20:1–22:1 2.5:1–3.5:1 GP, obere shiee Na-eweda nke ọma ma ọ bụrụ na ekpo oke ọkụ. Njikwa okpomọkụ ziri ezi
Iko juru / abrasive Kwa isi resin Kwa isi resin Ụdị ntọala + elu siri ike Geometry na-eso resin isi. Nkeelubụ ihe na-agbanwe: gaa bimetallic

Otu esi eji tebụl a:Ndị a bụ usoro ebipụta na mmalite, ọ bụghị nkọwapụta. Igwe gị, ọkwa gị, akụkụ gị, na mmepụta gị na-agbanwe ọnụọgụgụ. Onye na-emepụta ihe nkedo na-akwado geometry ikpeazụ megide ezigbo usoro gị. Ọ dịghị mgbe ị ga-esi na tebụl ọnụ ọgụgụ na-enweghị mkparịta ụka ahụ.

PP na PE: Semi-crystalline, Shear na-adịghị mma

Polyolefins bụ ikpe dị mfe. Ha na-anabata ịkwa akwa, gbazee na windo sara mbara ma na-agbaghara skru GP. Mkpakọ na-agafeghị oke na nke dị elu na-arụ ọrụ nke ọma, n'ihi na resins ndị a na-enweghị viscosity chọrọ mma shiee ka ọ gbazee nke ọma kama ịfefe na ọkara gbazere.

Push mmepụta ike na mkpa mgbidi, na ihe mgbochi ịghasa na-erite uru ya site na-ebunye a ọzọ gbazee zuru ezu n'otu ọsọ.

ABS na PS: Amorphous, Lelee Okpomọkụ Shear

Amorphous resins na-adị nro karịa ebe dị iche iche kama ịgbaze n'ebe dị nkọ. PS na-agba ọsọ na obere mkpakọ n'ihi na ọ na-agbaze ngwa ngwa. ABS chọrọ nlekọta ọzọ: ọ na-egosi streaks na splay mgbe ọ na-eweda ya ala, na ikpo ọkụ na-abụkarị ihe kpatara ya.

Ọ bụrụ na ahịrị akụkụ ABS na ebe ntọala gị dị ka nke ọma, chee na ọ ga-akpụ tupu ị na-enyo enyo nkụ. Oke mkpakọ na-eme ihe ike na resin amorphous nke na-enwe mmetụta ọkụ na-arụpụta ntụpọ nke ya.

PC na Injinia Plastics: Okpomọkụ dị elu, ogologo L/D

PC, naịlọn, PBT, na ndị ikwu ha na-agbaze elu ma na-eweda nso karịa nke ahụ. Ha chọrọ ịgbaze nke ọma, nke na-arụ ụka maka ogologo oge L / D, mana ha na-atakwa oge obibi, nke na-arụ ụka megide ijide agbaze na nnukwu gbọmgbọm.

Mkpebi ahụ dị ogologo L/D yana mkpakọ dị nro yana ogbunigwe nha nke ọma. Nweta nha ogbugba ahụ na-ezighi ezi na PC na okirikiri ihe onwunwe site na ọkụ ruo mgbe ọ na-acha odo odo, n'agbanyeghị etu ịghasa si dị mma.

PVC siri ike ma na-agbanwe agbanwe: Nguzogide nrụrụ dị oke egwu

Ihe niile dị n'elu gbasara PVC na-emetụta nhọrọ. PVC siri ike na-anọdụ ala na njedebe dị ala nke ma L / D na mkpakọ, n'ihi na oge na shear bụ ndị iro abụọ. Ọgwụgwọ elu ahụ aghaghị iguzogide corrosion, ọ bụghị naanị abrasion, nke ahụ na-agbanwe nhọrọ alloy n'ime gbọmgbọm bimetallic.

PET na POM: Shear dị ala, njikwa okpomọkụ ziri ezi

PET bụ hygroscopic. Mmiri dị n'ime gbazee na-eme ka ụdọ polymer na-eme ka agbụ polymer na-adaba, na-adaba viscosity dị n'ime, na-ahapụkwa ka ọ na-agbaji ma na-ekpo ọkụ mgbe igwe ahụ dị ka ọ na-arụ ọrụ nke ọma. Ghichaa resin nke ọma, mee ka shea dị ala, mee ka ebe obibi dị mkpụmkpụ, ma kọwaa ebe a na-egbu maramara ka nkwụnye ego ghara ịmalite.

POM na-anabata mkpakọ nkịtị mana ọ na-eweda ya nke ọma mgbe ọ na-ekpo oke ọkụ, na ngwaahịa mmebi ya dị ize ndụ. Ijikwa okpomọkụ na ọzụzụ oge obibi dị mkpa karịa geometry amamihe.

Ngwa ndị juru na iko na abrasive: Ahịrị 30%.

Nke a bụ iwu doro anya na ibe, ọ bụkwa ọnụọgụ, ọ bụghị mmetụta.Fiber Glass ruo 30%: nitrided 38CrMoAlA set na-ejikwa ya.Anyị na-ewu ma tụọ skru injection nitrided maka kpọmkwem nke ahụ, gbanyụọ ma kpasuo ya iwe, wee tinye gas-nitrided ruo 0.5-0.8 mm na 950-1050 HV.

N'elu iko 30%, ma ọ bụ nwere ihe mkpuchi ịnweta na ire ọkụ n'elu, elu ahụ ga-agbanwe.Ikpe nitrided bụ oyi akwa mgbasa, na ihe nchacha abrasive na-ebipụ ya ngwa ngwa karịa nchara dị n'okpuru kwesịrị.

Mgbe ahụ abimetallic ịghasa gbọmgbọmna-akwụsị ịbụ nkwalite wee bụrụ nkọwapụta ziri ezi: alloy siri ike fesa okirikiri zuru oke n'okirikiri ebe a na-eyi akwa ahụ, na-ewere ike dị n'ime ya ruo 62 HRC. Jiometry ka na-eso resin isi. Naanị elu na-agbanwe. Anyịbimetallic vs nitrided nduna-arụ ọrụ site na mgbagha ego.

Ụdị Barrel, Akụrụngwa, na Ọgwụgwọ Elu

gbọmgbọm ahụ adịghị ada nke ukwuu. Ọ na-emepe emepe, nwayọ, wee were ya were wepụta mmepụta gị. Ihe na elu na-ekpebi ogologo oge nke ahụ ga-ewe.

Ọkọlọtọ Nitrided Steel Barrel: Ngwa na oke

Nitriding na-agbasa nitrogen n'ime elu igwe, na-eme ihe siri ike. Anyị gas-nitride skru injection 38CrMoAlA anyị na 500–560 °C, na-emepụta oyi akwa nitrided 0.5–0.8 mm gbara ọkpụrụkpụ na 950–1050 HV. Nke ahụ na-ebuli nguzogide eyi 30-40% karịa igwe anaghị agwọ ya.

A na-agbanyụ ígwè isi ahụ ma na-ewe iwe nke mbụ, nke na-ebuli nkwụsi ike nke shear site na 50% n'onwe ya. Ọnụ, nzọụkwụ abụọ ahụ na-enye ndụ ọrụ ihe dị ka awa 10,000-20,000 na resin na-adịghị emebi emebi dị ka PE na PP.

Oke ya bụ omimi ikpe. Ozugbo abrasion ga-esi na oyi akwa nitrided, isi dị nro dị n'okpuru na-eyi ngwa ngwa. Anyị na-atụle skru injection nitrided anyị maka ihe mgbakwasa iko-fiber ruo 30% (PA gbakwunyere eriri iko, ọmụmaatụ). N'elu nke ahụ, ma ọ bụ na resins na-emebi emebi, ihe nitrided ahụ karịrị nke ahụ na elu ga-agbanwe.

Barrel Bimetallic: Mwube, Ọnụ, na Mgbe Ọ Na-akwụ ụgwọ

Otu gbọmgbọm bimetallic na-edobe ahụ alloy-steel ma na-etinye alloy dị iche iche n'ime oghere ahụ. N'elu gbọmgbọm anyị, anyị na-efesa alloy siri ike n'okirikiri nke mpaghara wears, na-ebute ike dị n'ime na 62 HRC.

Nke ahụ bụ ụdị nchebe dị iche site na nitriding. Ikpe nitrided bụ oyi akwa mgbasa nke a tụrụ n'ime iberibe milimita. Igwe ihe na-efe efe ma ọ bụ jikọtara ya bụ oyi akwa nke ọla dị iche iche, na ihe mkpuchi abrasive ga-agafe na ya niile.

A na-ahọrọ alloy maka ihe iyi egwu. Carbide-ọgaranya na tungsten-carbide n'elu na-eguzogide abrasion sitere na iko na ihe ndị na-ahụ maka ịnweta. Alloys na-ebu nickel na-eguzogide corrosion sitere na PVC na ogige ndị na-ere ọkụ. Họrọ alloy na-ezighi ezi ma kwụọ ụgwọ maka gbọmgbọm bimetallic nke na-edozi nsogbu na-ezighi ezi.

Ọ na-akwụ ụgwọ mgbe ọ bụla ndepụta gị na-emebi ma ọ bụ na-emebi emebi. Usoro mgbakọ na mwepụ dị mfe: ọ bụrụ na nhazi bimetallic na-adịru ọtụtụ ugboro ma ọ bụrụhaala na nitrided na ihe gị, ọnụ ahịa ịzụrụ dị elu na-ekewa na ọnụ ala dị ala kwa afọ, tupu ị gụọ akwụkwọ na oge nkwụsịtụ ị na-ezere.

Nkewa vs Monolithic Barrel: Mgbanwe vs nkenke

A na-eji otu ahụ arụpụta otu barel monolithic. Ọ na-ejide nkwụ ọtọ na nlebara anya kacha mma, ọ bụkwa ụkpụrụ maka ịkpụzi injection, ebe nkenke na-eme ka ọ bụrụ ihe na-agbanwe agbanwe.

gbọmgbọm ndị kewara ekewa na-agbakọta ọnụ site na ngalaba, nke na-enye ohere ka edochie akụkụ nke eyi na-ewepụghị gbọmgbọm ahụ dum, ma na-enye ohere ka edobe ọdụ ụgbọ mmiri ikuku n'ụzọ na-agbanwe agbanwe. Azụmahịa ahụ bụ nhazi: nkwonkwo ọ bụla bụ ohere maka nkwụsịtụ, na igwe injection adịghị agbaghara nke ahụ karịa ịgbakọta extruders.

Base Steel na Nhọrọ dị n'elu nke na-anọdụ na ya

38CrMoAlAbụ isi ígwè anyị igwe anyị injection kposara si, na ọ bụ ụlọ ọrụ ndabara maka ihe kpatara ya. Emebere kemịkalụ chromium-molybdenum-aluminium maka nitriding: aluminom na-etolite nitrides siri ike, kwụsiri ike n'okwu ahụ ebe isi na-esi ike.

Nchara nchara na-ebu ibu igwe. Elu n'elu ya na-eyi uwe, ọ bụkwa ebe ahụ ka ezigbo nhọrọ dị. Dị ka aemeputa gbọmgbọm ịghasaanyị na-enye oke elu zuru oke, onye ọ bụla na-aza ihe iyi egwu dị iche:

  • Nitriding- 0.5–0.8 mm oyi akwa na 950–1050 HV. Resins dị ọcha, eriri iko ruru 30%.
  • Bimetallic surfacing- alloy siri ike jikọtara na mpaghara ebe a na-eyi akwa, gbagoro ruo 62 HRC. Ọrụ abrasive na corrosive.
  • Tungsten carbide spraying- maka ikpe abrasion kacha sie ike.
  • Chrome plating- a ire ụtọ, ntọhapụ-enyi na enyi elu elu. Na-enyere aka na mgbanwe agba na ịrapara, ọ bụghị na abrasion dị arọ.
  • Igwe anaghị agba nchara- mgbe nguzogide corrosion ma ọ bụ ihe dị ọcha na-eduga ihe a chọrọ kama iyi.

Ntuziaka ihe ịghasa barel anyị na-atụnyere nchara isi n'uju.

Atụnyere ọgwụgwọ dị n'elu

Ihe / ọgwụgwọ Isi ike Yiri nguzogide Nguzogide corrosion Kachasị mma maka
38CrMoAlA, nitrided 950-1050 HV, 0.5-0.8 mm oyi akwa Ọ dị mma Na-agafeghị oke PE, PP, PS, ABS; eriri iko ruo 30%. Ihe ndabara akụ na ụba
Bimetallic surfacing Obere ruo 62 HRC Magburu onwe Ọ dị mma Glass juputara n'elu 30%, mineral juputara, regrind, ọrụ abrasive
Tungsten carbide spraying Dị elu Magburu onwe Ọ dị mma Okwu abrasion kacha sie ike
Nickel-base alloy surfacing Ahọpụtara n'otu nhazi Ọ dị mma Magburu onwe PVC, fluoropolymers, ọkụ retardants
Ihe mkpuchi chrome siri ike Ike, dị gịrịgịrị Na-agafeghị oke Ọ dị mma Ntọhapụ dị nro, mgbanwe agba dị mfe, mgbochi osisi
Igwe anaghị agba nchara Kwa ọkwa Na-agafeghị oke Magburu onwe Ngwa nrụrụ aka ma ọ bụ ịdị ọcha na-eduga

Ezipụta elu maka nri kachasị ruru unyi na ahịrị ga-agba ọsọ n'ezie, ọ bụghị nke kachasị ọcha. Ikowapụta maka ikpe dị ọcha bụ ụzọ a na-ahụkarị na ntọala ọhụrụ si anwụ n'isi.

Nlekọta: Otu esi enweta awa ọ bụla ihe nhazi ahụ nwere ike inye

Nlekọta anaghị atụgharị iyi. Ọ na-egbochi gị ịgbakwunye uwe a na-ezere n'elu ụdị a na-apụghị izere ezere, ọ na-enye gị data iji mee atụmatụ nnọchi kama imeghachi omume na ya.

Ndepụta nyocha oge niile

Ugboro ugboro Ihe ị ga-elele Ntak
Oge mgbanwe ọ bụla Agbazekwa okpomọkụ vs nkịtị, oge mgbake, nkwụsi ike n'ihe, ibu moto Ndị a akpafuola tupu ntụpọ apụta
Ihe ọ bụla ma ọ bụ agba na-agbanwe Sachaa nke ọma; nyochaa nchacha maka spek ojii ma ọ bụ ihe rụrụ arụ Speck pụtara ntụpọ nwụrụ anwụ ma ọ bụ mmebi ebe
Kwa ọnwa Chọpụta thermocouples na igwe ọkụ; lelee nri-akpịrị jụrụ oyi Ihe mmetụta na-efegharị efegharị na-esi nri ruo ọnwa na-ahụghị ya
Mgbe ọ bụla ịghasa pụtara Tụọ ụgbọ elu OD na ID gbọmgbọm n'ọnọdụ akara; nyochaa mgbanaka nlele Ihe nkedo apụtalarị. Nkeji iri nke nha bụ data efu
Ọ dịkarịa ala kwa afọ (ọrụ abrasive ma ọ bụ corrosive) Atụmatụ ịdọrọ: nha uwe zuru oke, nlele nhazi, dekọọ ọgụgụ Uwe ndị jupụtara, PVC na regrind na-etinye ngwa ngwa karịa resin dị ọcha

Usoro nhicha nke ọma mgbe ị na-agbanwe resins ma ọ bụ agba

Sachapụ tupu nkwụsị ọ bụla na mgbanwe ọ bụla, na-enweghị ihe ọ bụla maka ụbọchị ọrụ n'aka. Ihe hapụrụ ka ọ dị jụụ n'ime gbọmgbọm ahụ na-eweda ala, na-esi ya n'elu, ma laghachi ma emechaa dị ka specks ojii n'akụkụ onye ahịa.

Jiri ngwa nchacha azụmahịa maka mgbanwe agba, maka mmechi, na tupu ịgbanwee gaa na polymer nwere mmetụta ọkụ. Virgin PE ma ọ bụ PP na-ejikwa mgbanwe oge niile n'etiti ihe dakọtara. Resins dị elu dị ka PC na PMMA na-ejidesi ike ma chọọ nchacha ike karị.

Sachapụ tupu imechi, ọ bụghị naanị tupu ịmalite. Ihe ị hapụrụ na gbọmgbọm jụrụ oyi na-abụ nsogbu ị na-alụ na mmalite ọzọ.

Otu esi atụle mkpochapụ-na-Barrel

Nke a bụ nha na-atụgharị echiche ka ọ bụrụ eziokwu, ọtụtụ ụlọ ahịa na-amafe ya.

  1. Dọrọ ma hichaa ịghasa.Na-ekpo ọkụ, na ngwá ọrụ ọla ma ọ bụ ọla kọpa. Ọ dịghị mgbe ígwè scrapers, nke ebipụ mesoo elu nke ịghasa na-adabere.
  2. Kaa akara n'ọnọdụ nhan'ogologo na-arụ ọrụ: ndepụta, mgbanwe, na metering na opekempe.
  3. Tụlee ụgbọ elu ODya na micrometer dị n'èzí n'ọnọdụ ọ bụla, na-agụ akwụkwọ n'ọtụtụ ebe gburugburu gburugburu iji jide uwe na-enweghị isi.
  4. Tụta ID gbara gbọmgbọmya na ihe nlegharị anya na ọnọdụ dabara na omimi.
  5. Gbakọọ mkpochapụ radial:Wepụ ụgbọ elu OD site na ID akwụghị ụgwọ wee kewaa abụọ.
  6. Tulee megide ịbịaru ụlọma tinye ụbọchị na awa na-agba ọsọ ọ bụla.

Kọwaa nsonaazụ ya megide mkpochapụ mbụ, ọ bụghị megide ọnụọgụ zuru ụwa ọnụ. Iwu ụlọ ahịa bara uru: mgbe mkpochapụ toro ihe ruru okpukpu abụọ nke ọnụ ahịa ụlọ, ma ọ bụ mgbe mmepụta dara nke ọma n'otu ọsọ ahụ, malite ịhazi nhazi. Ntuziaka nha usoro nzọụkwụ anyị na-ekpuchi usoro ahụ n'uju.

Usoro nhicha na ihicha ụdị ngwakọta

Gwakọta ngwakọta ahụ na ọrụ ahụ. Mechanical (enweghị abrasive) na-asachapụ ahịhịa nwere nnukwu viscosity. Kemịkalụ na-ekpochapụ ihe mebiri emebi na carbon. Ihe na-ekpochapụ ụfụfụ na-agbasa ruo n'ebe nwụrụ anwụ nke mmiri na-asọ laminar na-atụfu.

Ogologo oge dị omimi na-adabere na resin. Ndị polymer na-ekpo ọkụ na-arụ ọrụ carbon ngwa ngwa ma chọọ nchacha miri emi ugboro ugboro. Ihe ọ bụla ị na-agba, debe oge ahụ n'usoro n'usoro kama ichere specks ojii ka ha hazie ya maka gị.

Mgbe Imezi vs Mgbe Dochie

Tulee ọnụ ahịa kwa afọ nke ọrụ, ọ bụghị mkpado ọnụahịa abụọ ahụ. Mwughachi nke na-efu ọkara mana ọ na-eweghachi otu ụzọ n'ụzọ atọ nke afọ bụ nhọrọ dị oke ọnụ na ngbanwe.

Ndozi dabere nrimgbe uwe bụ akụkụ na agafeghị oke, isi metal na-ada ụda, nke a bụ nke mbụ wughachi, na geometry ka dabara gị resin.

Nnọchi na-adabere nrimgbe corrosion abanyela n'ime miri emi, mgbe e wughachilarị ihe nkedo ahụ, mgbe ihe gị gbanwere na geometry ochie adịghịkwa adaba, ma ọ bụ mgbe nhazi ahụ bụ nha nkịtị nke ọnụahịa nnọchi ya na-anọdụ ala nso na nrụzi.

Ntuziaka nrụzi vs nnọchi anya na-ewepụta tebụl mkpebi zuru oke.

Nchekwa nke ọma na ijikwa ihe mpụtara screw Barrel

Ntọala mapụtara bara uru naanị ma ọ bụrụ na ọ kwụ ọtọ ma dị ọcha mgbe ịchọrọ ya. Chekwaa skru kwụ ọtọ na nkwado n'ogologo, anaghị adabere n'ọnụ ọnụ. Yiri ha nchara, kpuchie ha, ma debe mpempe akwụkwọ ahụ ma tụọ ọnụ ọgụgụ ndị siri ike na akụkụ ahụ.

Atụmatụ ntụgharị nke edobere mapụtarabara uru karịa ego ngwa ngwa ọ bụla, ọ fọrọ nke nta ka ọ bụrụ na ọ nweghị onye na-eweta ngwaahịa ga-agwa gị nke a. Zụta nnọchi tupu setịpụ ugbu a ada ada. Gbaa usoro ọhụrụ ahụ, ziga nke ochie maka iwughachi mgbe mmepụta na-aga n'ihu, ma debe ihe a rụgharịrị na shelf dị ka ihe nchekwa.

Ị nwere oge ntụgharị na oge efu na-enweghị atụmatụ, na nnọchi ọ bụla n'ọdịnihu na-eme na nhazi oge gị kama n'elekere abụọ nke ụtụtụ na Satọde. Atụmatụ a na-efu otu nnukwu ego ego na-arụ ọrụ ma na-akwụghachi ya na nke mbụ ndakpọ emeghị.

Ọ bụ usoro ka ọ bụ igwe? Ọnụ ụzọ Mkpebi

Nke a bụ ngalaba ọ nweghị onye asọmpi na-ede, ọ ga-azọpụtakwa gị oge karịa ka ejikọta ndị ọzọ ntuziaka a.

Mgbe ntụpọ ịkpụzi pụtara, ọtụtụ ndị otu na-eru maka ntọala igwe. Okpomọkụ, nrụgide azụ, ọsọ injection, oge ijide. Mgbe ụfọdụ, nke ahụ ziri ezi. Ma mgbe a na-eyi ihe mkpuchi plastik, ọ dịghị ntọala na-eweghachi usoro ahụ, izu na-apụkwa n'ime ọchụchọ na-enweghị ike ịga nke ọma.

Gbaa ọnụ ụzọ ámá a tupu ị metụ ebe ntọala ọzọ aka.

1. Ò nwere ihe gbanwere?Nza resin ọhụrụ, agba ọhụrụ, ogo regrind ọhụrụ, ebu ọhụrụ, ntọala mmadụ agbanweela? Ọ bụrụ ee, chụọ mgbanwe ahụ. Nke a bụ nsogbu usoro ruo mgbe egosipụtara na ọ bụghị.

2. Nrụ arụ pụtara na mberede, ma ọ bụ na-akpụ akpụ n'ime izu ole na ole?Atụ aka na mberede na mgbanwe ma ọ bụ ihe mebiri emebi. Nke nta nke nta na-eyi. Uwe anaghị abata n'otu abalị.

3. Nkwụkwụ ahụ ọ na-agbanwe agbanwe ka a na-agbapụ?Nkwadebe na-ekwekọghị ekwekọ bụ mgbanaka nlele na-ekwu okwu. Nyochaa ya tupu ihe ọ bụla ọzọ.

4. Mmepụta agbadala n'otu ọsọ ahụ, ma ọ bụ ogologo oge mgbake agbatịla?Ha abụọ na-arụtụ aka na mkpochapụ, nke pụtara ịghasa ma ọ bụ mgbọ egbe. Ntọala enweghị ike iweghachi mkpochapụ furu efu.

5. Ọ na-agbaze okpomọkụ na-arịgo na-agbanweghi agbanwe setpoint?Ihe nkedo a na-eme ka ọ dịkwuo ọkụ, na-emekarị n'ihi na ọ na-arụsi ọrụ ike megide nkwụsị nke eyi.

6. Species ojii na-alọghachi mgbe ọ bụla ihichachara?Ihe na-abanye n'ebe nwụrụ anwụ. N'ebe ochie, a na-eyikarị ebe ahụ nwụrụ anwụ nke na-ebunye agbaze agbaze.

Azịza atọ ma ọ bụ karịa "ee" n'ajụjụ 3 ruo 6 pụtara na igwe na-agwa gị na a na-eyi unit plasticizing. Kwụsị n'iji ya gee ntị. Dọrọ ịghasa wee tụọ ya.

Ntụle na-ewe otu awa. Ịchụso ntụpọ arụrụ arụ ọrụ site na ntọala na-ewe izu ole na ole, ọ dịghị mgbe ọ na-agbakọta, n'ihi na azịza ya anọghị na njikwa.

Ntuziaka nchọpụta nsogbu na tebụl ihe kpatara ya

Nrụrụ ọ bụla dị n'okpuru nwere ike si na usoro ma ọ bụ site na nrụnye igwe. Tebụl ahụ na-akpọ ahaịghasa na gbọmgbọmihe kpatara ya, n'ihi na nke ahụ bụ ọkara nke onye ọ bụla ọzọ na-ahapụ.

Nsogbu Mgbaàmà Mkpọsa / gbọmgbọm mgbọrọgwụ kpatara Omume mmezi
Black streaks/akara ọkụ Species gbara ọchịchịrị ma ọ bụ streaks na akụkụ ahụ; njọ mgbe nkwụsị Ihe e merụrụ emerụ na-abanye n'ime ebe a na-ekpuchi akwa ma ọ bụ ebe nwụrụ anwụ; gbagoro agbaji; elu ịghasa mebiri emebi Nchacha miri emi. Ọ bụrụ na specks laghachi, dọpụta wee nyochaa. Lelee maka akara akara na mkpochapụ eyighị. Dochie ma ọ bụrụ na ntọala ahụ bụ ihe na-ebufe
Nha ogbugba na-ekwekọghị ekwekọ / mkpirisi mkpirisi Agbapụ ibu arọ; ihe nkuku na-adịgasị iche ogbunigwe na agba Lelee mgbanaka anaghị emechi ya(kachasị nkịtị); ụgbọ elu na-eyi na-eme ka agbaze gbazee azụ; gbọmgbọrọ mgbọrọ arọn̄be Lelee mgbanaka nlele mbụ. Mgbe ahụ tụọ mkpochapụ. Ntọala agaghị edozi valvụ na-agbapụta anaghị eweghachi
Agbazekwa okpomọkụ spiking Ezi agbaze okpomọkụ n'elu setpoint; ihe discoloring Oke shiee site na oke mkpakọ na-ezighi ezi; mkpochapụ na-eyi na-eme ka ịghasa na-arụ ọrụ siri ike; thermocouple furu efu Chọpụta thermocouples. Lelee ọsọ skru na nrụgide azụ. Ọ bụrụ na geometry ezighi ezi maka resin, kposara bụ ihe ndozi
Iweghachite nwayọ / ogologo plasticizing Oge mgbake na-agbatị; oge okirikiri na-eto Mwepu na-eyi na-ebelata arụmọrụ mgbapụta; mbipụta ngalaba ndepụta; geometry na-ezighi ezi maka resin Lelee nri-akpịrị jụrụ oyi na pellet nri. Mgbe ahụ tụọ nkwụsịtụ megide eserese ahụ
Ibu moto na-ebili / nrụgide azụ Amps moto na-arị elu na mmepụta mgbe niile; torque mkpu Ịkpọsa na-adọkpụ n'ime olulu ahụ (malignment, gbagọọ skru); oke itucha; ihe na-ewu ewu ewu ewu Lelee nhazi n'usoro ma kpochie nha anya. Ihe nkedo agbagọ na-eyi otu akụkụ nke mkpọ ma ga-emebikwa gbọmgbọm ọhụrụ
Mmebi ihe / ngbanwe agba Na-acha odo odo, splay, kenkuwa, isi Oge obibi ogologo oge (obere obere maka gbọmgbọm); shisie oke ike; ntụpọ nwụrụ anwụ na-ejide ihe Lelee nha ogbunigwe na ike gbọmgbọm. Belata shiee. N'elu resins na-ekpo ọkụ na-ekpo ọkụ, ihe nkedo dị ala nwere ike ịbụ naanị ihe ndozi
Ihe na-adịghị agbaze / ihe siri ike na akụkụ Nkịta siri ike; ntụpọ dị ka oghere; adịghị ike tụrụ Ike mgbaze na-ezughị ezu: L/D dị mkpụmkpụ, mkpakọ na-ezighi ezi, mmepụta gafere ihe ịghasa nwere ike gbazee, ma ọ bụ ihe mgbochi. Belata mmepụta ma ọ bụ kwalite gaa na skru mgbochi. Ọ bụrụ na etinyere ntọala ahụ, ọ nweghị ntọala na-enweta agbaze ahụ
Agba streaking / adịghị mma mgbasa Agba na-enweghị isi; masterbatch adịghị agbasa Enweghị ngalaba ngwakọta; eyi ịghasa Ịgwakọta emezighituri; ịghasa na-ezighi ezi maka ogige jupụtara ma ọ bụ nwere agba Ezipụta ngalaba agwakọta (Maddock ma ọ bụ pin). Chọpụta na ịghasa abụghị naanị ike agwụla mbụ

Black Streaks ma ọ bụ ọkụ Mark

polymer rụrụ arụ na-arahụ ebe ma na-agbaji iberibe. A na-eyi ebe ezoro ezo nke ọma, ebe mgbanaka akara, mgbanaka nlele mebiri emebi, na ebe ọ bụla nwụrụ anwụ ebe mmiri na-asọ mpi.

Buru ụzọ kpochapụ miri emi. Ọ bụrụ na specks ahụ lọta azụ ka emechara nke ọma, ihe ahụ abụghị naanị ihe fọdụrụ. A na-arụpụta ya mgbe niile site n'otu ntụpọ dị na igwe gị, ma ịkwesịrị ịdọrọ ịghasa wee chọta ya.

Nha Mgbo na-ekwekọghị ekwekọ ma ọ bụ mkpụmkpụ mkpirisi

Lelee mgbanaka tupu ị metụ ntọala. Mgbe valvụ na-adịghị alaghachi azụ kwụsịrị akara, gbazee na-agbanarị azụ n'oge ịgba ntụtụ, na ogbunigwe ahụ chere na ọ tụrụ abụghị ogbugba nke ebu ahụ na-enweta.

Ihe nrịba ama bụ nkwụ. Usoro na-agbanwe agbanwe na-ejide ihe nhịahụ na-adịgide adịgide. Mgbe ihe nkuku na-awagharị ka a gbagburu, agbaze na-aga ebe ọ na-ekwesịghị.

Agbazekwa okpomọkụ ma ọ bụ oke elu

Jiri nyocha tụọ agbaze n'ezie kama ịtụkwasị obi na ntọala ndị ahụ. Ọ bụrụ na agbaze n'ezie na-agba ọsọ nke ọma n'elu mpaghara ahụ, oke okpomọkụ na-abịa site na shear, ọ bụghị site na eriri.

Ọkụ na-ekpo ọkụ na-ebili mgbe mkpakọ dị oke ike maka resin, mgbe ọsọ ọsọ dị oke elu, mgbe nrụgide azụ dị oke, na mgbe ihe nkedo na-eyi na-agbasi mbọ ike ịkwaga otu ihe ahụ.

Iweghachite Screw Screw / Ogologo oge Plasticizing

Malite na hopper. Ịchịkọta pellets, akpịrị nri na-ekpo ọkụ nke ukwuu, na nri ezughị ezu na-ajụ oyi niile na-eme ka agụụ ahụ gbatịa ma gbatịa mgbake, ma ọ dịghị nke ọ bụla n'ime ha bụ ntụpọ.

Ọ bụrụ na nri nri dị mma na mgbake ka na-adị nwayọ, tụọ nkwụsịtụ ahụ. Ihe nkedo nke tụfuru arụmọrụ mgbapụta ya iji eyi na-ewe ogologo oge iji mejupụta otu ogbugba ahụ, oge okirikiri na-egosipụtakwa ya.

Ibu moto na-ebili ma ọ bụ nrụgide azụ

Ịkwalite amps na mmepụta mgbe niile pụtara ihe na-eguzogide. Ihe nkedo agbagọ na-adọkpụ n'ime oghere bụ ihe dị ize ndụ: ọ na-eyi otu akụkụ nke gbọmgbọm ahụ, na ihe nkedo ọhụrụ arụnyere megide ihe na-adịghị mma na-eyi otu ụzọ n'otu oge.

Lelee nzizi na nhazi tupu ị tụọ ihe ọ bụla. Uwe nwere otu akụkụ bụ akara mkpisiaka.

Mmebi ihe ma ọ bụ ngbanwe agba

Ihe abụọ kpatara ya na-achịkwa: ihe ahụ dị oke ọkụ, ma ọ bụ na ọ na-ekpo ọkụ ogologo oge. Nke abụọ bụ nke ndị mmadụ na-atụ uche.

Mgbọ nke dị nnọọ obere maka gbọmgbọm ahụ na-agbaze na-anọdụ ala n'okirikiri mgbe ọ gachara, na-esi nri nwayọ ruo mgbe ọ na-acha odo odo. Ọnweghị ihe mkpọsa na-edozi obere mkpụbelata n'ime nnukwu gbọmgbọm buru ibu. Dezie dayameta nke skru, ma ọ bụ bugharịa ọrụ ahụ na igwe pere mpe.

Otu esi atụọ ọdụ ihe ngbanwe screw Barrel

Ọ dịghị onye asọmpi na-ekpuchi nke a, ọ bụkwa akụkụ nke ndị na-azụ ahịa chọrọ n'ezie. Ma ị na-enye iwu site na OEM ma ọ bụ site na onye nweere onwe yaịghasa barrel factory, otu ozi ahụ na-eme ka okwu ahụ pụta ìhè.

Akụkụ na nkọwapụta ị ga-enyerịrị

  • Ụdị igwe na ihe nlereanya.Foto dị n'ụdị aha ezuola iji kwado akụkụ nrịgo na njedebe mbanye.
  • Dayameta nke ịghasa na nha L/D,site na eserese ma ọ bụ tụọ ozugbo.
  • The resin, na ndochi ọdịnaya.Nke a na-eme ka nchara isi na ọgwụgwọ elu karịa ihe ọ bụla ọzọ na ndepụta ahụ.
  • Nha ogbugba na okirikiri ebumnuche,yabụ enwere ike imezi geometry karịa ka e depụtaghachiri ya.
  • Ihe osise, ma ọ bụ ihe nlele eyi.Nke ọ bụla na-arụ ọrụ. Enwere ike tụọ akụkụ yitere wee rụgharịa geometry zuru ezu.
  • Kedu ihe mere n'oge ikpeazụ.Zipu ụkpụrụ ejiji na akụkụ ahụ. Mbelata akụkụ dị nro na-ekwu abrasion. Pitting na-ekwu corrosion. Uwe otu akụkụ na-ekwu nhazi, nke ịghasa ọhụrụ agaghị edozi.

Ihe ikpeazụ ahụ bụ nke ndị na-azụ ahịa na-echefu, ọ bụkwa ya na-akwụsị ịzụrụ akwụkwọ nke ọdịda.

OEM-Match vs Custom Design: Uru na ọghọm

Egwuregwu OEMna-emepụtagharị geometry mbụ. Ọ bụ oku ziri ezi mgbe ịghasa mbụ dabara na usoro gị wee gwụ ya. Enwere ike ịkọ amụma, kwenye n'aka na eserese ahụ, enweghị nkwado usoro.

Nhazi omenalana-agbanwe geometry ka ọ dabara ihe ị na-agba taa. Ọ bụ oku ziri ezi mgbe usoro ahụ kwagara na nkedo ahụ emeghị: ị gbakwunyere regrind, gbanwee gaa na ọkwa zuru ezu, gbanwee ihe mgbaru ọsọ mmepụta, ma ọ bụ ihe nkedo mbụ ahụ ejighị resin gị nke ọma.

Ịtụ ihe egwuregwu OEM mgbe usoro ahụ gbanwere na-emepụtaghachi nsogbu ahụ na ígwè ọhụrụ. Ịtụ nhazi omenala mgbe nke mbụ dị mma na-agbakwụnye ọnụ ahịa na nkwụghachi ụgwọ n'efu. Ụdị ejiji na-agwa gị ọnọdụ ị nọ na ya.

Ihe ị ga-atụ anya mgbe ị na-esi na China nweta

Oge ndu na-adabere na geometry, ọgwụgwọ elu, yana ma eserese ọ dị. Rịọ ya na ederede site na ntinye okwu gị, wee jụọ ihe elekere na-amalite na: nkwenye nke eserese, ma ọ bụ usoro ịzụrụ ihe. Ha abụghị otu ụbọchị, na ihe dị iche na-abụkarị otu izu.

Ihe atọ kwesịrị ịtụle tupu ịmee:

  • Mgbe mmepụta amalite.Reverse-ingineering a eyi sample na-agbakwụnye oge tupu otu mgbawa ebipụ. Ihe osise na-ewepụ nzọụkwụ ahụ.
  • Ihe ọgwụgwọ elu na-agbakwụnye.Bimetallic surfacing na carbide spraying bụ usoro usoro dị iche iche nwere kwụ n'ahịrị nke ha.
  • Ibu oke osimiri, iche iche.Ọ bụghị n'oge ụzọ nrụpụta, ọ bụkwa ọnụ ọgụgụ na-eju ndị na-azụ ahịa oge mbụ anya.

Nkwupụta nke onwe anyị na-apụta ìhè site na imewe: anyị na-enye ọnụ ahịa echere na-ekpuchi ngwaahịa ahụ, mbupu, na nlekọta na-aga n'ihu, n'ihi ya ọ dịghị ihe ga-achọpụta ma emechaa. Ị ga-enweta nkwupụta ahụ n'ime awa 12.

Mee atụmatụ gburugburu oge ntụzịaka site na iji ngbanwe a mapụtara mapụtara nke akọwara na mbụ. Otu iwu nyere iwu site na ụgbọ mmiri wear log na nhazi oge gị. Ntọala nyere iwu site na ụgbọ mmiri ndakpọ megide elekere, site na ikuku, na ọnụ ahịa ọ dịghị onye na-enwe mmasị ịkọwa.

Usoro nnabata nke ọma yana ntụle nyocha

Ndị a bụ ndenye ego na-ekewa ezigbo ndị na-ebubata ya na nke dị ọnụ ala. Rịọ ha n'edemede tupu ị tinye iwu, wee nyochaa ha mgbe nhazi ahụ rutere:

  • Dayameta dị n'èzí n'ọtụtụ ebe n'akụkụ ụgbọ elu ọ bụla
  • Obere dayameta na cylindricity
  • Isi ike dị n'elu dị ka atụrụ uru(HV ma ọ bụ HRC), ọ bụghị nkọwa katalọgụ
  • Omimi ikpe nitrided, ma ọ bụ ihe omimi alloy n'elu bore bimetallic
  • Concentricity na kwụ ọtọ
  • Ọkpụkpụ elu (Ra)
  • Isi ọkwa nchara, kwadoro

Isi ike na ịdị omimi nke ikpe bụ ihe abụọ kachasị mkpa, na nke abụọ na-adịkarị nwayọọ belata. Okpokoro nitrided na 950-1050 HV na 0.5–0.8 mm dị omimi bụ nkọwapụta ị nwere ike ijide onye na-ebubata ya. "Nitrided" n'onwe ya abụghị.

Ọ bụrụ na ngụta daa nke ukwuu n'okpuru ndị ọzọ, jụọ ihe nchara dị na otú omimi nke ọgwụgwọ ahụ si agba. Nke ahụ bụ ihe fọrọ nke nta ka ọ bụrụ mgbe niile ebe ọdịiche ahụ na-ezo, ma ị na-akwụghachi ya na uwe mbụ.

Ihe nlegharị anya anyị zuru oke na-anọdụ n'usoro ntụzịaka nke ịghasa barrel omenala.

Chọrọ ihe ngbanwe ma ọ bụ ogbugba ogbugba omenala? Zipu ụdị igwe gị, eserese, ma ọ bụ ihe nlere eyi. Anyị na-ehota n'ime 12 awa.

Nweta Quote Screw Barrel

Ajụjụ a na-ajụkarị

Ajụjụ: Ogologo oge ole ka ogbunigwe na-akpụzi skru barrel na-adịru?

A: Na resin na-adịghị emebi emebi dị ka PE na PP, skru injection 38CrMoAlA nitrided anyị na-agba ihe dị ka awa 10,000-20,000. Ngwakọta juru iko, PVC, na regrind dị arọ belata nke ahụ, yana ogologo dabere na ọdịnaya na mmepụta ihe. Adịla ọsọ elekere na olileanya: tụọ. Lelee ụgbọ elu OD ma were ID megide eserese ihe owuwu opekata mpe otu ugboro n'afọ n'ọrụ abrasive, wee banye usoro a. Usoro a, ọ bụghị ọnụ ọgụgụ awa, na-agwa gị mgbe ị ga-atụnye usoro na-esote.

Ajụjụ: Gịnị bụ ụkpụrụ nchapụta n'etiti ịghasa na gbọmgbọm?

A: Ọ dịghị otu ọnụ ọgụgụ, n'ihi na mkpochapụ akpịrịkpa na ịghasa dayameta. Ụkpụrụ isi mkpịsị aka ụlọ ọrụ maka nhazi ọhụrụ bụ ihe dị ka 0.001 inch nke radial mkpochapụ n'otu akụkụ maka inch ọ bụla nke dayameta skru, yabụ ala ịghasa 60mm dị nso 0.06 mm kwa akụkụ. Ihe osise ụlọ gị bụ ikike. Dịka oke ọrụ bara uru, mgbe mkpochapụ atụpụtara toro ruo ihe dị ka okpukpu abụọ nke ọnụ ahịa ihe nrụpụta, ma ọ bụ mmepụta agbadala nke ọma n'otu ọsọ ahụ, hazie nnọchi anya.

Ajụjụ: Enwere m ike iji otu ịghasa maka resin dị iche iche?

A: N'ime ezinụlọ, ee. Ihe nkedo ebumnuche izugbe na-eji PE, PP, PS, na ABS anabata nke ọma, nke mere ndị na-ewu igwe ji ebu ya dị ka ọkọlọtọ. N'ofe ezinụlọ, mba. Ihe nkedo GP na PVC siri ike na-emebi ihe ahụ ma mebie ígwè ahụ. Ihe GP skru na naịlọn jupụtara ugo na-agwụ ngwa ngwa. Na ịghasa nha maka otu olu ogbugba enweghị ike ịrụ ọrụ nke na-eji obere akụkụ nke gbọmgbọm eme ihe na-esighi ihe. Ọ bụrụ na resins gị gafere oghere ndị ahụ, ị ​​ga-achọ ihe karịrị otu skru, ma ọ bụ skru emebere maka ikpe kacha sie ike.

Ajụjụ: Kedu ka m ga-esi mara ma ọ bụrụ na eyi skru na-akpụzi injection m?

A: Igwe na-agwa gị na mbụ, na micrometer na-akwado ya. Lezienụ anya maka ọdịda mmepụta n'otu ọsọ nke mgbake, ịgbatị oge mgbake, gbazee okpomọkụ na-arị elu na ntọala agbanweghị, specks ojii na-alọghachi mgbe ihichachara, na ịgbagharị nha nha. Nke ọ bụla n'ime ihe ndị ahụ na-akwado ịdọrọ nkesa. Wee were micrometer tụọ OD ụgbọ elu ma jiri ihe nlegharị anya were were were were tụọ OD, n'ọnọdụ dakọtara, wee tulee mkpochapụ radial megide eserese ahụ. Mgbaàmà na-atụ aro; nha na-akwado.

Ajụjụ: Gịnị bụ bmetallic screw barrel na kedu mgbe m chọrọ otu?

A: Otu gbọmgbọm bimetallic na-edobe ahụ alloy-steel ma na-etinye alloy siri ike karịa n'ime oghere ahụ. N'elu gbọmgbọm anyị, anyị na-efesa alloy siri ike gburugburu gburugburu ebe a na-eyi uwe, na-ebute ike dị n'ime na 62 HRC. Ahịrị dị mfe ise:eriri iko ruo 30% na-arụ ọrụ nke ọma na ntọala 38CrMoAlA nitrided. Ihe karịrị iko 30%, nke nwere ihe mkpuchi ịnweta ma ọ bụ ire ọkụ, ma ọ bụ na resin na-emebi emebi, gaa bimetallic. Ikpe nitrided bụ oyi akwa mgbasa nke 0.5–0.8 mm, na ihe ndo dị arọ na-esi na ya rie ogologo oge tupu nchara dị n'okpuru agwụchaa.

Ajụjụ: Ime ịghasa ọ na-emetụta ogo akụkụ na ịkpụzi injection?

A: Kpọmkwem, na karịa ọtụtụ usoro ntọala. Screw geometry na-ekpebi ka ihe ahụ na-agbaze kpamkpam, ka agbaze agbaze si dị, etu agba na nchacha si gbasa nke ọma, yana ka ogbugba ahụ si na-agbanwe agbanwe. Agbazeghị, streaks, splay, mweda, na ogbugbu dịgasị iche iche na-achọpụta azụ na screw designs ma ọ bụ screw yi opekata mpe ka ha na-alaghachi na njikwa. Mgbe ntụpọ na-emegide mgbanwe ntọala ọ bụla ị na-eme, geometry ma ọ bụ eyi na-abụkarị ihe kpatara ya.

Ajụjụ: Gịnị bụ ihe dị iche n'etiti ihe nkedo injection na extrusion kposara?

A: Ihe nkedo extrusion na-atụgharị na-aga n'ihu na nfuli na-agbaze n'ihu na-akwụsịghị. Ihe nkedo ntụtụ na-arụ ọrụ abụọ: ọ na-atụgharị ka ọ na-eme ka égbè mee plastik, wee kwụsị ịgbagharị ma na-ebugharị n'ihu dị ka onye na-agbapụta ịgbanye ya. Ihe na-emeghachi omume ahụ bụ ihe kpatara skru injection na-ebu mgbanaka nlele n'ọnụ ọnụ, yana ihe kpatara ha ji agba ọsọ L/D dị mkpụmkpụ, nke na-abụkarị 18: 1 ruo 25: 1, karịa skru extrusion. Akụrụngwa na-anọdụkwa na gbọmgbọm ịgba ntụtụ n'etiti gbaa, nke na-eme ka oge obibi na nha nha dị oke egwu.

Ajụjụ: Onye na-emepụta ihe nkedo gbọmgbọm nwere ike iṅomi mkpọsa na-enweghị eserese?

A: Ee. Mbupu akụkụ eyi na geometry nwere ike tụọ ma wughachi ya: dayameta, akụkụ akụkụ, omimi ọwa, na nha dabara na njedebe mbanye. Anyị na-ejide skru injection ruo ±0.001 mm. Otu ịdọ aka ná ntị kwesịrị ikwu: ihe nkedo na-eyi ihe dị obere karịa ka ọ hapụrụ ụlọ ọrụ mmepụta ihe, ya mere ekwesịrị iji dochie anya n'ebumnobi mbụ ahụ karịa ka ọ dị nha. Zipu ihe mkpuchi na akụkụ ahụ, na ịghasa ọhụrụ ahụ akọwapụtara megide ọdịda kama iketa ya.

Mmechi

Atọ echiche na-ebu dum ndu.

Nhọrọ na-esote resin.Geometry (L/D, nha mkpakọ, ụdị ịghasa) dabara ka polymer gị si agbaze. Ngwọta dị n'elu dabara ka ndepụta gị si dị unyi. Resin dị ọcha na-agba ọsọ nke ọma na nitrided 38CrMoAlA. Nri abrasive na nke na-emebi emebi chọrọ eriri bimetallic, na ịkọwapụta ikpe dị ọcha bụ ụzọ a na-ahụkarị n'usoro ọhụrụ na-anwụ n'isi.

Nlekọta na-azụta afọ, na data na-azụta atụmatụ.Sachaa tupu nkwụsị ọ bụla, jiri ọla kọpa dị ọcha karịa ígwè, ma tụọ nkwụsịtụ mgbe ọ bụla ịghasa pụtara. A wear log tụgharịrị "ọ na-eyi?" n'ime "olee mgbe ọ ga-agafe akara?", Nke bụ ihe dị iche n'etiti mgbanwe mgbanwe na nkwụsịtụ.

Nyochaa igwe tupu i dozie usoro a.Mgbe mmepụta dara ada, okirikiri gbatịa, ihe nkuku na-awagharị, ma ọ bụ specks laghachiri mgbe ihichachara, ngalaba plastik na-ekwu okwu. Ntọala enweghị ike iweghachite mkpochapụ furu efu ma ọ bụ mechie mgbanaka nlele eyi. Dọrọ ịghasa wee tụọ ya.

Nanhaiya arụla skru na gbọmgbọm ihe karịrị afọ iri abụọ ma na-ejere ndị ahịa 500+ ozi n'ụwa niile. A na-eji 38CrMoAlA na-emepụta skru injection anyị, menyụọ ma na-ewe iwe, wee mee gas-nitrided na 500–560 °C ruo ihe dị ka 0.5–0.8 mm na 950–1050 HV, na-ejide ya na nnabata nke ±0.001 mm, wee tụọ ya maka awa 00-1000-1000-100-100-100-100-100-100-1000-1000-1000-100-100-100-100-100-100-100-10 hours. resins. N'ebe nri ahụ siri sie ike, anyị na-efesa alloy siri ike gburugburu gburugburu ebe a na-eyi akwa ma were ike ime ya gaa 62 HRC.

Tupu ị nye iwu, ndị injinia anyị na-arụ ọrụ site na paramita gị: dayameta, akụkụ akụkụ, omimi ọwa, yana nhọrọ ihe dị n'etiti 38CrMoAlA na alloy duplex. Ndụmọdụ ahụ bụ n'efu, na ntinye nke na-esote gụnyere ngwaahịa, mbupu, na ụgwọ mmezi a na-atụ anya ya, yabụ na ọ nweghị ihe ga-apụta mgbe e mesịrị nke na-anọghị na ibe ahụ.

Mgbe nnyefe, ndị ọrụ nka anyị na-akwado nrụnye na inye ọrụ, akwụkwọ ikike na-aga nkwekọrịta (na-abụkarị otu afọ ruo afọ abụọ), na okwu ọ bụla mgbe ire ere na-enweta nzaghachi n'ime awa 24 yana ngwọta n'ime 48.

Zitere anyị ụdị igwe gị, resin na nsogbu ị na-achọ idozi. Ị ga-enwe nkọwapụta na see okwu n'ime awa iri na abụọ.

Gwa anyị igwe gị, resin gị, na ihe na-adịghị mma n'oge ikpeazụ. Anyị ga-akọwapụta nhazi nke na-edozi ya, ọ bụghị nke na-emegharị ya.

Kpọtụrụ Nanhaiya maka nkwupụta
Akụkọ metụtara
Hapụ m ozi
X
Anyị na-eji kuki iji nye gị ahụmịhe nchọgharị ka mma, nyochaa okporo ụzọ saịtị na hazie ọdịnaya. Site na iji saịtị a, ị kwenyere na ojiji anyị ji kuki. amụma nzuzo
JụNabata