Aluminom-Plastic Panel Single Screw
  • Aluminom-Plastic Panel Single ScrewAluminom-Plastic Panel Single Screw

Aluminom-Plastic Panel Single Screw

The Aluminom-Plastic Panel Single Screw ozugbo na-ekpebi àgwà nke isi oyi akwa, mmepụta nrụpụta na ọnụ ahịa. Ngwakọta ahụ na-ekpo ọkụ, ịkwachaa, gbazee na homogenized na otu ịghasa extruder, na-eme ka otu agbaze edo edo. Gbaa mbọ hụ na nkwụsi ike nke ịdị mma.

Nkọwa mmepụta

1. A na-ekpebi dayameta nke Aluminom-Plastic Panel Single Screw dị ka obosara nke osisi aluminom-plastic na mmepụta chọrọ. Nha a na-ahụkarị gụnyere Φ65mm, Φ90mm, Φ120mm, Φ150mm, wdg.

2. A na-emeso elu nke otu ihe nkedo maka ịdị nro dị elu, a na-ehichapụkwa ọwa mmiri na-asọ asọ iji gbochie nkwụsịtụ na mmebi nke ihe ndị ahụ, si otú a na-ezere ịmepụta ntụpọ ojii.

3. The pụrụ iche aluminum-plastic osisi kenha ịghasa imewe atụmatụ a ịghasa isi na a pinion mixing ngalaba. Isi nke ịghasa na-ewere ọdịdị torpedo ma ọ bụ okirikiri iji zere akụkụ ndị nwụrụ anwụ ma gbochie ihe ịrapara na ire ere.

Aluminum-Plastic Panel Single ScrewAluminum-Plastic Panel Single ScrewAluminum-Plastic Panel Single Screw

Ngwa ngwaahịa

Oke

Nkọwa

Ịghasa dayameta

Nkọwa ndị a na-ahụkarị gụnyere 35mm, 45mm, 65mm, 75mm, 85mm, 90mm, etc. Dịka ọmụmaatụ, mgbe ị na-edozi ọkpọkọ PVC, a na-eji screw 65mm eme ihe n'ọtụtụ ebe ka ọ na-enweta ezigbo nguzozi n'etiti mmepụta na ike oriri.

Ogologo Ogologo ruo na dayameta (Ratio L/D)

Ọ na-adịkarị site na 20:1 ruo 30:1. Maka plastik nwere mmetụta ọkụ dị ka PVC, nha L / D na-abụkarị n'etiti 20: 1 na 25: 1. Nke a na-eme ka plasticization zuru oke ma na-ebelata oge obibi nke ihe dị na gbọmgbọm iji belata ihe ize ndụ nke ire ere.

Oke mkpakọ

Ọ na-adakarị n'etiti 3.5:1 na 4.5:1. Oke mkpakọ ka ukwuu na-eme ka plastik zuru oke na mkpirisi ihe PVC.

Omimi Channel Screw

Ọwa ịghasa dị ntakịrị nke na-emighị emi, karịsịa na ngalaba mita. Nhazi a na-ebelata oge obibi nke ihe ma na-ebelata ohere nke ire ere.

Ọnụọgụ nke Mpaghara kpo oku na oyi

Ọdịiche dabere na skru dayameta na nkọwa akụrụngwa, na-abụkarị site na mpaghara 5 ruo 6. Dịka ọmụmaatụ, onye na-ekpochapụ otu ihe nkedo nwere dayameta nke 65mm nwere ike ịnwe mpaghara kpo oku na oyi 6 iji mee ka njikwa okpomọkụ dị na nke ọ bụla.

Ịghasa Ọsọ

Ọ dị mkpa ka edoziri ọsọ ọsọ dịka dayameta skru na ihe mmepụta chọrọ. Maka ịghasa φ65mm, mgbe ị na-emepụta ọkpọkọ nwere mgbidi mgbidi 3mm, a na-achịkwa ọsọ a na-atụ aro n'ime oke nke 25-35rpm.

Ike mbanye

Ejikọtara ya na dayameta skru na mmepụta. Ọmụmaatụ, otu ịghasa extruder na a 65mm ịghasa dayameta a na-enwe a mbanye ike nke 45-90kw.

Okpomọkụ na-arụ ọrụ

The okpomọkụ nke nri ngalaba bụ n'ozuzu 160-170 ℃, agbaze ngalaba bụ 180-190 ℃, na anwụ isi ngalaba bụ 175-185 ℃.

Njirimara Ngwaahịa Na Ngwa

1. Na NHY otu ịghasa gbọmgbọm maka alu-plastic panel, Otu oru oma mgbochi-ụdị agwakọta ngalaba ana achi achi zuru ezu agbaze. Gbaa mbọ hụ na okpomọkụ na-agbaze bụ otu, ma gbasasịa ndị na-acha agba, ọkụ retardants na ihe mgbakwunye ndị ọzọ iji kwe nkwa na agba na-agbanwe agbanwe na ịrụ ọrụ nke mpempe akwụkwọ ahụ.

2. Iji gbochie ike corrosiveness nke ire ere retardant, elu nke otu ịghasa na-emeso ya na a dual alloy nke ike tungsten carbide siri ike iji hụ na ogologo oge akụkụ nkwụsi ike. ogwe ọkpọ ọkpọ, ogwe ndị nwere ụdị pụrụ iche, wdg.

Aluminum-Plastic Panel Single ScrewAluminum-Plastic Panel Single Screw
Aluminum-Plastic Panel Single ScrewAluminum-Plastic Panel Single ScrewAluminum-Plastic Panel Single Screw
Zipu ajụjụ
Ozi kọntaktị
Nabata na webụsaịtị anyị! N'ihi na ajụjụ banyere anyị ngwaahịa ma ọ bụ pricelist, biko hapụ email gị ka anyị na anyị ga-aka n'ime 24 awa.
X
Anyị na-eji kuki iji nye gị ahụmịhe nchọgharị ka mma, nyochaa okporo ụzọ saịtị na hazie ọdịnaya. Site na iji saịtị a, ị kwenyere na ojiji anyị ji kuki. amụma nzuzo
JụNabata